Problem 1: Coating Defects


Conventional films are divided into two types: coated and uncoated, and the reasons for ink drop caused by film coating defects are also divided into two cases: For coated film materials, if the surface coating has poor firmness, it will lead to ink adhesion. Poor; and uncoated film materials, due to the poor bonding fastness between the surface layer and the ink, often cause ink drop.


For ink droplets caused by coating defects, it can be solved by the following methods: use surface layer varnish printing treatment to protect the ink surface and prevent ink droplets; the surface layer is corona treated, and the corona dyne value on the surface of the material should not be lower than 38mm/ m, the dyne value lower than 36mm/m will directly affect the fastness of the ink; the surface layer should be primed or an enhancer with strong ink adhesion should be used (the mixing ratio is about 3%). ), can also improve the ink adhesion of the film surface; some sub-surface synthetic paper materials are not suitable for testing with 3M tape because the surface coating has certain paper coating characteristics.


Problem 2: Tension


For the corona-treated film material on the printing surface, in order to achieve good ink wettability, the dyne value usually needs to be above 38mm/m, if it is lower than 36mm/m, it is prone to ink drop problems; The dyne value will gradually decrease over time, and there will be problems with the printing ink. The essence of the problem is tension.


For the ink droplets caused by this situation, there are the following solutions: use a satellite rotary machine with online corona function for online corona treatment to improve the surface energy of the film material; use a batch printing machine for surface primer coating treatment, In order to improve the adhesion of surface printing; when the dyne value decreases, corona treatment is required during printing, but the size of the dyne value cannot fully represent the adhesion between the ink and the surface material. Generally, the decay period of the dyne value is 3 months to 6 months, so it is recommended to minimize the long-term storage of raw materials in inventory.


Finally, it is recommended to use ink with higher adhesion, and it is recommended to consult the ink supplier.


Problem 3: Ink Drying and Tension


Ink drying and tension can also cause ink to drip during the printing process. Specifically divided into: the ink layer is too thick, resulting in incomplete drying; insufficient UV lamp energy, lamp aging, lamp reflector aging, resulting in insufficient drying and curing of the UV lamp, and the ink layer is not dry; excessive drying of the ink, causing the material Deformation, the formation of ink layer peeling off.


This ink drop problem can be solved in three ways:


One is to use dark ink and thin printing, commonly known as reducing the amount of ink. For example, spot inks can be paired with darker volumes. The amount of ink in regular printing is small, which can achieve the effect of proofing. At the same time, the output power of the UV lamp can be increased. , reduce the printing speed and increase the exposure time of the UV lamp to achieve the drying effect. This solution is suitable for old batch or satellite rotary machines and old UV lamp solutions.


2. Check whether the UV lamp is aging and clean the reflector. Generally, the service life of domestic UV lamps is about 500-1000 hours, and the service life of imported lamps is about 1000-2500 hours. For details, please refer to the actual use. It is recommended that the printing factory clean the UV lamp every six months or so to ensure normal use.


Third, reduce the output power of the UV lamp. The specific operation is the general printing house printing operation. The first few sets of colors in the color sequence are mostly logos or small characters. The required light is limited. Advanced over-irradiation is not allowed because the thermal energy absorbed by the film material is limited. Excessive exposure will cause the film material to curl, deform, become brittle, and reduce ink adhesion. You can follow the principle of using low-grade UV lamps first and then high-grade lamps.


Question 4: Ink Matching


Finally, how well the ink and material are matched will also contribute to the droplets to some extent. For example, the molecular tension of the ink is too large to form a uniform ink layer on the surface of the substrate; or the use of ink models that have passed the shelf life or inferior domestic brand inks will cause ink loss.


In the above cases, you can use inks that match the printing materials, such as film-specific inks and light-fast and light-fast inks (consult the ink manufacturer for specific consultation); for expired inks, you need to check the situation before printing. Do a printing test, or print some simple characters or small logo patterns, as well as some low-end products; to print large-area solid and full-screen dot-and-line patterns, it is recommended to use inks with good brands and high adhesion (such as Hanghua Ink, etc.).


Summary of Ink Drop Influence Factors


Through the above analysis, we can summarize eight reasons for ink droplets:


1. The surface coating fastness of the coating material is poor;


2. The uncoated film material has poor bonding fastness with the ink after printing;


3. The dyne value is low. For the corona-treated film material on the printing surface, to achieve good ink wettability, the dyne value usually needs to be above 38mm/m;


4. The dyne value decreases, the printing surface is corona-treated film material, the dyne value gradually decreases with time, and the decline period is 3-6 months;


5. The printing ink layer is too thick and the UV lamp power is insufficient, resulting in insufficient curing of the ink layer;


6. The ink tension is too large to form a uniform cured ink layer on the surface of the printing material;


7. Use expired ink or inferior domestic ink;


8. The ink is over-irradiated and over-dried.